Baja cor tahan korosi, uga disebut baja tahan karat, nuduhake baja cast alloy sing nuduhake resistensi kuat kanggo korosi ing macem-macem media korosif tartamtu utawa lingkungan ing ngendi korosi lan faktor mekanik ana bebarengan.
Tampilan cepet kanggo Austenitic Stainless Steel | |
Komposisi Kimia Utama | Cr, Ni, C, Mo, Cu, Si, Nb, Ti |
Kinerja | Non-magnetik, kateguhan dhuwur, plastisitas dhuwur, kekuatan kurang |
definisi | Baja tahan karat kanthi struktur austenitik ing suhu kamar |
Kelas Perwakilan | 304, 316, 1.4310, 1.4301, 1.4408 |
Kemampuan mesin | Adil |
Weldability | Umume apik banget |
Panggunaan Khas | Mesin Pangan, Hardware, Pengolahan Kimia ... lsp |
Baja tahan karat nduweni kandungan kromium minimal 10,5%, dadi luwih tahan kanggo lingkungan cairan korosif lan oksidasi. Iku banget tahan karat lan tahan nyandhang, menehi machinability banget, lan kondhang kanggo tampilan estetis sawijining. Casting investasi stainless steel minangka "tahan karat" nalika digunakake ing lingkungan cair lan uap ing ngisor 1200 ° F (650 ° C) lan "tahan panas" nalika digunakake ing ndhuwur suhu iki.
Baja tahan karat Austenitiknuduhake stainless steel karo struktur austenitic ing suhu kamar. Baja tahan karat Austenitik minangka salah siji saka limang kelas baja tahan karat kanthi struktur kristal (bebarengan karo feritik, martensitik, duplex lan presipitasi hardened). Ing sawetara wilayah, baja tahan karat austentite uga diarani baja tahan karat seri 300. Nalika baja ngemot babagan 18% Cr, 8% -25% Ni, lan babagan 0,1% C, nduweni struktur austenit sing stabil. Baja tahan karat kromium-nikel Austenitik kalebu baja 18Cr-8Ni sing misuwur lan baja seri Cr-Ni dhuwur sing dikembangake kanthi nambahake isi Cr lan Ni lan nambahake Mo, Cu, Si, Nb, Ti lan unsur liyane ing basis iki. stainless steel Austenitic non-Magnetik lan wis kateguhan dhuwur lan plasticity, nanging kekuatan kurang, lan iku mokal kanggo ngiyataken liwat transformasi phase. Mung bisa dikuwatake kanthi kerja sing adhem. Yen unsur kayata S, Ca, Se, Te ditambahake, iku nduweni sifat machinability apik.
Austenitic stainless steel uga bisa gawé casting. Kanggo nambah fluiditas baja molten lan nambah kinerja casting, komposisi campuran saka baja cast kudu diatur kanthi nambah isi silikon, nggedhekake sawetara isi kromium lan nikel, lan nambah wates ndhuwur belerang unsur impurity.
Austenitic stainless steel kudu ngalangi-solusi dianggep sadurunge nggunakake, supaya minangka kanggo nggedhekake solusi ngalangi saka macem-macem precipitates kayata carbide ing baja menyang matrik austenite, nalika uga homogenizing struktur lan mbusak kaku, supaya minangka kanggo mesthekake resistance Korosi banget lan sifat mekanik. Sistem perawatan solusi sing bener yaiku pendinginan banyu sawise dadi panas ing 1050 ~ 1150 ℃ (bagean sing tipis bisa uga digawe adhem). Suhu perawatan solusi gumantung saka tingkat alloying baja: Molybdenum-free utawa low-molybdenum baja gelar kudu luwih murah (≤1100 ℃), lan gelar alloyed luwih kayata 00Cr20Ni18Mo-6CuN, 00Cr25Ni22Mo2N, etc. 1080~1150) ℃).
Austenitic 304 stainless steel plate, kang ngandika nggawa kuwat anti-teyeng lan resistance karat, lan wis plasticity banget lan kateguhan, kang trep kanggo stamping lan mbentuk. Kanthi Kapadhetan saka 7,93 g / cm3, 304 stainless steel punika stainless steel banget umum, uga dikenal minangka 18/8 stainless steel ing industri. Produk logam tahan suhu dhuwur lan nduweni sifat pangolahan sing apik, mula digunakake kanthi akeh ing industri lan industri dekorasi perabot lan industri panganan lan medis.
Kelas Setara saka Stainless Steel | |||||||
Kategori | AISI | W-stoff | DIN | BS | SS | UNE / IHA | UNI |
Baja tahan karat martensit lan feritik | 420 C | 1.4034 | X43Cr16 | ||||
440 B/1 | 1.4112 | X90 Cr Mo V18 | |||||
- | 1.2083 | X42 Kr 13 | - | 2314 | F.5263 | - | |
403 | 1.4000 | X6Cr13 | 403 S 17 | 2301 | F.3110 | X6Cr13 | |
(410S) | 1.4001 | X7 Kr 14 | (403 S17) | 2301 | F.3110 | X6Cr13 | |
405 | 1.4002 | X6 KrAl 13 | 405 S 17 | - | F.3111 | X6 KrAl 13 | |
416 | 1.4005 | X12 CrS 13 | 416 S 21 | 2380 | F.3411 | X12CrS13 | |
410 | 1.4006 | X 10 Kr 13 | 410 S21 | 2302 | F.3401 | X12Cr13 | |
430 | 1.4016 | X6 Kr 17 | 430 S 17 | 2320 | F.3113 | X8Cr17 | |
420 | 1.4021 | X20 Cr 13 | 420 S 37 | 2303 | F.3402 | X20Cr13 | |
420F | 1.4028 | X30 Cr 13 | 420 S 45 | (2304) | F.3403 | X30Cr13 | |
(420) | 1.4031 | X39Cr13 | 420 S 45 | (2304) | F.3404 | - | |
431 | 1.4057 | X20 CrNi 17 2 | 431 S 29 | 2321 | F.3427 | X16CrNi16 | |
430F | 1.4104 | X12 CrMoS 17 | - | 2383 | F.3117 | X10CrS17 | |
434 | 1.4113 | X6 CrMo 17 | 434 S 17 | 2325 | - | X8CrMo17 | |
430Ti | 1.4510 | X6 CrTi 17 | - | - | - | X6CrTi17 | |
409 | 1.4512 | X5 CrTi 12 | 409 S 17 | - | - | X6CrTi12 | |
Baja Tahan Karat Austenitik | 304 | 1.4301 | X5 CrNi 18 9 | 304 S 15 | 2332 | F.3551 | X5CrNi18 10 |
305 | 1.4303 | X5 CrNi 18 12 | 305 S 19 | - | - | X8CrNi19 10 | |
303 | 1.4305 | X12 CrNiS 18 8 | 303 S 21 | 2346 | F.3508 | X10CrNiS 18 09 | |
304L | 1.4306 | X2 CrNiS 18 9 | 304 S 12 | 2352 | F.3503 | X2CrNi18 11 | |
301 | 1.4310 | X12 CrNi 17 7 | - | 2331 | F.3517 | X12CrNi17 07 | |
304 | 1.4350 | X5 CrNi 18 9 | 304 S 31 | 2332 | F.3551 | X5CrNi18 10 | |
304 | 1.4350 | X5 CrNi 18 9 | 304 S 31 | 2333 | F.3551 | X5CrNi18 10 | |
304LN | 1.4311 | X2 CrNiN 18 10 | 304 S 62 | 2371 | - | - | |
316 | 1.4401 | X5 CrNiMo 18 10 | 316 S 16 | 2347 | F.3543 | X5CrNiMo17 12 | |
316L | 1.4404 | - | 316 S 12/13/14/22/24 | 2348 | X2CrNiMo17 12 | ||
316LN | 1.4429 | X2 CrNiMoN 18 13 | - | 2375 | - | - | |
316L | 1.4435 | X2 CrNiMo 18 12 | 316 S 12/13/14/22/24 | 2353 | - | X2CrNiMo17 12 | |
316 | 1.4436 | - | 316 S 33 | 2343 | - | X8CrNiMo 17 13 | |
317L | 1.4438 | X2 CrNiMo 18 16 | 317 S 12 | 2367 | - | X2CrNiMo18 16 | |
329 | 1.4460 | X3 CrNiMoN 27 5 2 | - | 2324 | F.3309 | - | |
321 | 1.4541 | X10 CrNiTi 18 9 | 321 S 12 | 2337 | F.3553 | X6CrNiTi18 11 | |
347 | 1.4550 | X10 CrNiNb 18 9 | 347 S 17 | 2338 | F.3552 | X6CrNiNb18 11 | |
316Ti | 1.4571 | X10 CrNiMoTi 18 10 | 320 S 17 | 2350 | F.3535 | X6CrNiMoTi 17 12 | |
309 | 1.4828 | X15 CrNiSi 20 12 | 309 S 24 | - | - | X16 CrNi 24 14 | |
330 | 1.4864 | X12 NiCrSi 36 16 | - | - | - | - | |
Duplex Stainless Steel | S32750 | 1.4410 | X 2 KrNiMoN 25 7 4 | - | 2328 | - | - |
S31500 | 1.4417 | X 2 CrNiMoSi 19 5 | - | 2376 | - | - | |
S31803 | 1.4462 | X 2 KrNiMoN 22 5 3 | - | 2377 | - | - | |
S32760 | 1.4501 | X 3 KrNiMoN 25 7 | - | - | - | - | |
630 | 1.4542 | X5CrNiCNb16-4 | - | - | - | - | |
A564/630 | - | - | - | - | - | - |
Bahan Ferrous lan Non-ferrous kanggo Casting Investasi, Proses Casting Lilin Ilang:
- • Wesi Gray: HT150, HT200, HT250, HT300, HT350; GJL-100, GJL-150, GJL-200, GJL-250, GJL-300, GJL-350; GG10~GG40.
- • Wesi Ulet utawa Wesi Nodular: GGG40, GGG50, GGG60, GGG70, GGG80; GJS-400-18, GJS-40-15, GJS-450-10, GJS-500-7, GJS-600-3, GJS-700-2, GJS-800-2; QT400-18, QT450-10, QT500-7, QT600-3, QT700-2, QT800-2;
- • Baja Karbon: AISI 1020 - AISI 1060, C30, C40, C45.
- • Baja Paduan: ZG20SiMn, ZG30SiMn, ZG30CrMo, ZG35CrMo, ZG35SiMn, ZG35CrMnSi, ZG40Mn, ZG40Cr, ZG42Cr, ZG42CrMo...etc ing panyuwunan.
- • Stainless Steel: AISI 304, AISI 304L, AISI 316, AISI 316L, 1.4401, 1.4301, 1.4305, 1.4307, 1.4404, 1.4571 lan bahan stainless steel liyane.
- • Kuningan, Tembaga Abang, Perunggu utawa logam campuran basis Tembaga liyane: ZCuZn39Pb3, ZCuZn39Pb2, ZCuZn38Mn2Pb2, ZCuZn40Pb2, ZCuZn16Si4
- • Bahan Liyane miturut syarat unik sampeyan utawa miturut standar ASTM, SAE, AISI, ACI, DIN, EN, ISO, lan GB
Langkah-langkah ing proses utawa casting lilin sing ilang yaiku:
- • Nggawe pola lilin utawa replika
- • Sprue pola lilin
- • Investasi pola lilin
- • Ngilangi pola lilin kanthi ngobong (ing tungku utawa ing banyu panas) kanggo nggawe cetakan.
- • Force molten logam pour menyang jamur
- • Cooling lan Solidification
- • Copot sprue saka castings
- • Rampung lan polish castings investasi rampung




Perlakuan Panas saka AISI 316 Stainless Steel Casting:
Kalor nganti minimal 1900 ° F (1040 ° C), tahan wektu sing cukup, mateni banyu utawa adhem kanthi cepet kanthi cara liya. AISI 316 padha karo CF8M / F316 lan Standar Cina 0Cr17Ni12Mo2. AISI 314 minangka modifikasi bantalan molibdenum saka paduan AISI 304 lan padha karo baja tahan karat CF8M tempa. Ing ngarsane molybdenum nambah resistance karat umum lan resistance kanggo pitting dening klorida. Paduan iki digunakake ing kahanan sing rada asam lan alkalin lan kanggo nangani asam sitrat, oksalat lan fosfat.